Might consider requiring only lotions that have been tested to and passed
the IPC-TM-650 "copper mirror" test method designed to test flux induced
corrosion.
Gene Felder
[log in to unmask]
-----Original Message-----
From: Dieselberg, Ron [SMTP:[log in to unmask]]
Sent: Monday, July 08, 2002 12:40 PM
To: [log in to unmask]
Subject: Re: [TN] Question on Handling - Contamination 3.4.3
<< File: ATT00004.html >> Carl, our policy is, "Use only the hand lotion
that the company supplies. Do
not use other hand creams or lotions."
Ron Dieselberg
Trainer/Auditor
CMC ELECTRONICS
CINCINNATI
[log in to unmask]
-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Monday, July 08, 2002 14:21 PM
To: [log in to unmask]
Subject: [TN] Question on Handling - Contamination
3.4.3
Technetters,
Please put your legal hats on and help with a statement
that
would cover the
"Hand Lotion" issue in 3.4.3.
I am trying to get a statement into our company policy and
am getting some
resistance on the proper wording. I am open to suggestions
on proper wording
of a clear statement that eliminates the possibility of
someone using an
unacceptable hand cream (i.e. Avon, Jergens (all good hand
creams, but not
on circuitry), etc.). Any examples would be appreciated.
Would like to make
this a non-issue soon.
Thanks,
Carl Barnes
Production Process Analyst
480-968-6790
extension: 4236
Page At: 602-201-1435
------------------------------------------------------------------------
----
-----
Technet Mail List provided as a free service by IPC using
LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send
e-mail
to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm
for additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
------------------------------------------------------------------------
----
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|