Might consider requiring only lotions that have been tested to and passed the IPC-TM-650 "copper mirror" test method designed to test flux induced corrosion. Gene Felder [log in to unmask] -----Original Message----- From: Dieselberg, Ron [SMTP:[log in to unmask]] Sent: Monday, July 08, 2002 12:40 PM To: [log in to unmask] Subject: Re: [TN] Question on Handling - Contamination 3.4.3 << File: ATT00004.html >> Carl, our policy is, "Use only the hand lotion that the company supplies. Do not use other hand creams or lotions." Ron Dieselberg Trainer/Auditor CMC ELECTRONICS CINCINNATI [log in to unmask] -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Monday, July 08, 2002 14:21 PM To: [log in to unmask] Subject: [TN] Question on Handling - Contamination 3.4.3 Technetters, Please put your legal hats on and help with a statement that would cover the "Hand Lotion" issue in 3.4.3. I am trying to get a statement into our company policy and am getting some resistance on the proper wording. I am open to suggestions on proper wording of a clear statement that eliminates the possibility of someone using an unacceptable hand cream (i.e. Avon, Jergens (all good hand creams, but not on circuitry), etc.). Any examples would be appreciated. Would like to make this a non-issue soon. Thanks, Carl Barnes Production Process Analyst 480-968-6790 extension: 4236 Page At: 602-201-1435 ------------------------------------------------------------------------ ---- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ------------------------------------------------------------------------ ---- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------