Werner,
Package looks visual fine on the reflowed boards hence my comment. Perimeter
joints visually look fine too. Per our test folks, it passes when they apply
the thump pressure on the BGA. This package is TBGA package.
re,
ken patel
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Monday, January 22, 2001 3:09 PM
To: [log in to unmask]
Subject: Re: [TN] Urgent...Open underneath the BGA
Hi Ken,
When you say "BGA package looks sturdy to handle the heat", what to you
mean?
BGAs with Cu heat spreader sure look sturdy, but can warp like potato chips
when heated.
Werner Engelmaier
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|