Werner,



Do you think (have data) that Pb tends to segregate at GB?



Regards,



Vladimir

SENTEC

------Original Message------

From: Werner Engelmaier

Sender: TechNet

To: [log in to unmask]

ReplyTo: TechNet E-Mail Forum

ReplyTo: Werner Engelmaier

Subject: Re: [TN] SAC & LEAD (Pb) CONTAMINATION

Sent: Dec 8, 2009 16:04



Hi Lee,

First Q: What is the source of this info?

Second: We have seen the incredible difference some of this 

trace-additives can make; so why not Pb. But this is really 

'undiscovered' territory.

Werner



-----Original Message-----

From: Lee Whiteman <[log in to unmask]>

To: [log in to unmask]

Sent: Tue, Dec 8, 2009 3:52 pm

Subject: [TN] SAC & LEAD (Pb) CONTAMINATION



Today, I read where if you added 0.5% Lead (Pb) into SAC, that the 

fatigue life would be reduced from 18,670 to 8,089.



Question: How would the fatigue life react with Lead (Pb) levels in SAC 

ranging from 0.0% (Baseline) through 1.0%? Is it a linear relationship 

or exponential relationship?



Thanks again.



Lee Whiteman, PMP

Senior Member Engineering Staff

L-3 Communications East

Telephone: (856) 338-3508

FAX: (856) 338-2906

E-Mail: [log in to unmask]



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------







SENTEC

11 Canadian Road, Unit 7.

Scarborough, ON M1R 5G1

Tel: (416) 899-1882

Fax: (905) 882-8812

www.sentec.ca

ATOM RSS1 RSS2