TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, David Tremmel <[log in to unmask]>
Date:
Mon, 24 Mar 2008 07:26:10 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
A<00a001c88ac2$ed8eb3e0$c8ac1ba0$@com>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (70 lines)
Socially transmitted disease and an old term soldering temperature duration, which related to time an iron was held to a joint or dwell in a solder fountain or contact time across the wave.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: Thursday, March 20, 2008 12:45 PM
To: [log in to unmask]
Subject: [TN] J-STD-33 and 33B.1

Hello TechNet gurus,

 

In a former life I was responsible for a BGA reballing operation and the
bake-in / bake-out times and temps was based on J-STD-33.  A typical leaded
PBGA was MSL 3 and we baked it for 24 hrs at 125°C yaddah, yaddah, yaddah.

 

According to J-STD-33B.1 it appears that the same component now has a bake
time of 27 hrs and not 24 hrs?  I understand the same PBGA going from a lead
to a lead-free package and from MSL 3 to MSL 4.  But why were the 3 hours
added between the 2 standards?

 

Also, I realize that STD is short for STanDard, but doesn't STD also mean
something else?

 

 

Thank you in advance for your replies.

 

 

Thank you,

 

David Tremmel

Value Recovery

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2