TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"<Jason M. Smith>" <[log in to unmask]>
Date:
Thu, 25 Jun 1998 16:07:38 -0400
Content-Type:
text/plain; charset=us-ascii
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (29 lines)
Experts, I am currently getting alot of failures at my functional tester.
At my post solder station, I am noticing strings of dross across the pins
of connectors.  We are having to dedross the pot daily....for a no-clean
process and inerted atmosphering, I think this is a bit extreme.  Once, an
operator managed to accidently put stencil cleaner in the flux....could
this cause a reaction unable to be corrected without dumping the pot and
cause excess dross.  I initially thought we had too much exhaust drawing
all nitrogen away from the wave.  Our flux manufacturer did analyis and has
determined that it's not the residues left which is causing my bridges at
functional.  Is a type 'C' solder analysis going to tell me anything of
significance to my problem from any of your experiences?  Any
suggestions????

Jason Smith
Process Materials Engineer
Lexmark Electronics

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2