TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
peter blokhuis <[log in to unmask]>
Date:
Tue, 28 Aug 2001 14:00:53 -0700
In-Reply-To:
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (98 lines)
I would add to this that the rate of oxidation to
stannic tin is dependent on the temperature of the
solution, so we keep ours around 70F.

Peter Blokhuis



--- "<Rudy Sedlak>" <[log in to unmask]> wrote:
> Sean:
>
> The murky solution is due to Stannic Tin, and since
> Stannic is converted from
> Stannous, by oxidation, there really is only two
> ways it can happen.
>
> The first obvious one is by reaction with Oxygen in
> the air.  This is
> certainly a factor always, but if you are entraining
> a lot of air with the
> eductors, you could raise the rate of this occurring
> many times.
>
> The other way it can occur is by excessive (anode)
> current density..so if you
> are using bar anodes ask if they are being
> replenished as often as they
> should be.
>
> The next question to ask is, what is the effect of
> STannic Tin in the plating
> bath, and the answer, as in all of PCB's is "That
> depends"...
> The oxide dissolves a helluva lot faster in alkaline
> solutions than the
> metal, and this COULD cause/allow (apparent) etching
> of the Tin at a much
> faster rate, and thus could cause apparent
> overetching, or perhaps pitting of
> the Copper.
>
> And the other thing that can happen is that this
> Stannic Oxide in the deposit
> can dissolve into the photoresist stripper.  Some
> resist strippers lack the
> key ingredient in them to prevent immersion plating
> back on to the Copper,
> and thus you can wind up with copper partly unetched
> due to the presence of
> immersion Tin.  This is especially the case if you
> are attempting to strip in
> a tank, although, in this day of insane tight
> dimension specs, I have seen it
> cause problems in spray stripping as well.
>
> Filtration of Stannic is EXTREMELY difficult due to
> the extreme fine particle
> size (the brightener/leveler in the Tin plating is a
> surfactant that causes
> extreme small particles to form).
>
> Rudy Sedlak
> RD Chemical
>
>
---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC
> using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the
> following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line
> Resources & Databases > E-mail Archives
> Please visit IPC web site
> (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
>
---------------------------------------------------------------------------------


__________________________________________________
Do You Yahoo!?
Make international calls for as low as $.04/minute with Yahoo! Messenger
http://phonecard.yahoo.com/

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2