1. Other specifications MIL-I-46058c, IPC CC830 and IEC1086 but remember
these are test specifications not application. I do not know of an
application standard.
We do have application sheets covering dip, spray and brush, if you send be
your address I have them sent to you.
2. Bubbles in solvent based coatings is normally due to solvent entrapment
caused by a coating thickness greater then 0.003", you should withdrawal at
2" to 3" per minute, this is best done with automatic equipment.
3. Contact Don Hague at W.M. Hague on 781-275-8400 who should be able to
help with a small dipping system and air drying system.
Best Regards
David Greenman
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|