1. Other specifications MIL-I-46058c, IPC CC830 and IEC1086 but remember these are test specifications not application. I do not know of an application standard. We do have application sheets covering dip, spray and brush, if you send be your address I have them sent to you. 2. Bubbles in solvent based coatings is normally due to solvent entrapment caused by a coating thickness greater then 0.003", you should withdrawal at 2" to 3" per minute, this is best done with automatic equipment. 3. Contact Don Hague at W.M. Hague on 781-275-8400 who should be able to help with a small dipping system and air drying system. Best Regards David Greenman [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################