     There are many other considerations which should be weighed 
     prior to accepting these boards. First any Fabricator should 
     not make judgements on the acceptability of product which 
     doesn't meet a Customers specifications. The Customer, in 
     most cases, has reasons for his specifications. There could 
     be a height issue, component lead issues, UL agency, designed 
     in capacitance ect.... The best course of action is to notify 
     your Customer and discuss the variation.


______________________________ Reply Separator _________________________________
Subject: Re[2]: Assy/Fab: PCB Thickness
Author:  [log in to unmask] at Internet
Date:    6/3/96 12:38 PM


     I believe that the additional thickness will do very little to the 
     electrical performance nor its reliability. Your vendor did a poor job 
     in material selection and his up front engineering stackup. The 
     problems in assembly would be if the axial leaded devices do not have 
     long enough leads to properly protrude through the board for good 
     solder connection practices.
     
     
______________________________ Reply Separator _________________________________
Subject: RE: Assy/Fab: PCB Thickness
Author:  [log in to unmask] at SMTPpost1 
Date:    6/3/96 11:51 AM
     
     
Dear Technet,
     
First, please bare with me my inexperience in PCB fabrication. 
One of our customer's requirement for their PCB's thickness, ranges from 
1.55 to 1.60 mm. However, our PCB manufacturer supplies us the thickness 
ranges from 1.70 to 1.77 mm.
     
As our customer requires this board to be assemblied and shipped urgently, 
I would like to know 
     
a.      how this happens , 
b.      whether this difference in thickness will affect the assembly process, 
c.      whether it will affect the reliability and the electrical performance.
     
as to decide to use this board or to delay the shipment..
     
I thanks you in advance ... 
     
     
Poh Kong Hui
Nera Electronics 