Hello everyone !
We are experiencing here some solder quality problem after our solder
reflow process. The quality of the solderability of components
spcecifically the QFP IC's was not that good. The formation of the
solder fillet was convex on the IC leads which sometimes looks to be
grainy and sometimes it looks to be that the solder paste has
suddenly stop from flowing to its desired area. We already checked
the profile parameters of our reflow process and it is within the
specs limit of the solder paste that we are using. Do you think that
the thawing time of the solder paste have something to do with this
kind of problem ? Thank you in advance to anyone that could give a
solution to this problem.
Regards,
Ricky
Electronics Assemblies, Inc. Phils.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|