TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Fri, 25 May 2007 13:33:06 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
Werner

The discussion was focused on immersion silver. This was first introduced in 94 in the UK which was long after Jack's work which I recall was plated silver. Are you aware of any documented occurrences embrittled immersion silver solder joints?

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389 
  ----- Original Message ----- 
  From: [log in to unmask]<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> ; [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Friday, May 25, 2007 12:45 PM
  Subject: Re: [TN] Silver Embrittlement?


  Hi Lee,
  For the Ag-embrittlement you have to ggo to the IEEE Compliant Lead Task Force, that Jack Balde chaired, reports; Au-embrittlement has been around since the 60's 

  Werner



  **************************************
  See what's free at http://www.aol.com<http://www.aol.com/>. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2