TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 4 May 2010 16:35:05 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Subject:
From:
Ioan Tempea <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
A<A63B17202AB54B26ADB6D95202EAA523@dmcfarlandPC>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (70 lines)
Don,

I haven't met yet solderballing in SMT process that I could not eliminate through proper stencil apertures (reduction, homeplating, etc.).

Regards,

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] 
W | www.digico.cc

N'imprimer que si nécessaire - Print only if you must


-----Message d'origine-----
De : Don McFarland [mailto:[log in to unmask]] 
Envoyé : May-04-10 4:20 PM
À : [log in to unmask]
Objet : [TN] Does solder mask specified create solder balls?

Hi Technetters, 

I was asked to perform a DOE to determine if there was a correlation
between solder mask types and the rate at which we see solder balls
develop on the PWB surface. I searched through the archives and found a
few articles from the mid-90s about this topic, but couldn't glean
anything exciting from the posts reviewed. I am wondering if anyone knows
of a good source of information that addresses this topic or has anything
that would be useful for us. 

We have made a number of changes to other process variables (e.g. stencil
apertures, solder pastes, paste viscosity, profiles, etc) and have seen
good results, but we wanted to rule this out as a causal factor as well. 

Any help is greatly appreciated!

Don McFarland
  

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2