TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 6 May 2010 03:00:56 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Nigel Burtt <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="windows-1252"
Content-Transfer-Encoding:
quoted-printable
From:
Nigel Burtt <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Clearly flux and process set-up are influencing factors, but once all available 
adjustments have been made, we too found that the biggest improvement 
available was to specify matt finish soldermasks. The glossier finishes 
apparently soften slightly at soldering temperatures and allow solder balls to 
adhere to the surface - the rougher surface texture of a matt finish 
discourages the balls from staying. We also found matt finish masks helped 
shift stubborn solder bridges caused by PCB design. The "extra-matte" version 
of the Coates Imagecure resist gave us the best results, but no doubt others 
are equally good.

<http://www.sunchemical.com/products/electronic_materials/imagecure>

<http://www.axoncircuit.com/downloads/Coates.pdf>

Nigel

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2