In some cases, thinner is better.  For example, when you look at solder
joint reliability, the thinner the board, the more reliable the joint is.
Why?  Because thinner board can flex and not constraining the solder joint
as much as the thicker board.

However, the laminate is stretching the copper barrel in the case of PTH
symmtrically - no flexing.  The more copper on the barrel means more
material bearing the load.

You are right about not relying solely on intuition.  That's why we also
run experiments, e.g. thermal cycling, to verify these theories.

Mason

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2