TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Date:
Tue, 8 Dec 2009 17:29:37 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (94 lines)
Hi Vladimir,
I have seen no such data—and what I think is not relevant. what i know 
would be, but i do not know anything about this.
Werner

-----Original Message-----
From: vladimir Igoshev <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>; Werner Engelmaier 
<[log in to unmask]>
Sent: Tue, Dec 8, 2009 4:31 pm
Subject: Re: [TN] SAC & LEAD (Pb) CONTAMINATION

Werner,

Do you think (have data) that Pb tends to segregate at GB?

Regards,

Vladimir
SENTEC
------Original Message------
From: Werner Engelmaier
Sender: TechNet
To: [log in to unmask]
ReplyTo: TechNet E-Mail Forum
ReplyTo: Werner Engelmaier
Subject: Re: [TN] SAC & LEAD (Pb) CONTAMINATION
Sent: Dec 8, 2009 16:04

Hi Lee,
First Q: What is the source of this info?
Second: We have seen the incredible difference some of this
trace-additives can make; so why not Pb. But this is really
'undiscovered' territory.
Werner

-----Original Message-----
From: Lee Whiteman <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Dec 8, 2009 3:52 pm
Subject: [TN] SAC & LEAD (Pb) CONTAMINATION

Today, I read where if you added 0.5% Lead (Pb) into SAC, that the
fatigue life would be reduced from 18,670 to 8,089.

Question: How would the fatigue life react with Lead (Pb) levels in SAC
ranging from 0.0% (Baseline) through 1.0%? Is it a linear relationship
or exponential relationship?

Thanks again.

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text 
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: 
http://listserv.ipc.org/archives
Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



SENTEC
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2