TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 10 Mar 2008 23:06:00 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; format=flowed; charset="Windows-1252"; reply-type=original
From:
Parts/Attachments:
text/plain (185 lines)
Water is absorbed by acetone = faster concrete reaction, no wonder they like 
your acetone = faster money = risk of  lower quality ?
Inge


----- Original Message ----- 
From: "Terry L. Munson" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, March 11, 2008 1:47 PM
Subject: Re: [TN] SV: [TN] disposal of alcohol/DI water solution


> All I know is that they pick up my IPA and use it to burn when making 
> concrete for the highway construction.
>
> Terry
> Sent from my Verizon Wireless BlackBerry
>
> -----Original Message-----
> From: "Stadem, Richard D." <[log in to unmask]>
>
> Date:         Tue, 11 Mar 2008 15:33:43
> To:[log in to unmask]
> Subject: Re: [TN] SV: [TN] disposal of alcohol/DI water solution
>
>
> Terry,
> That sounds dangerous. I once had a friend who got really drunk and passed 
> out in the mix trough. You haven't really had a hangover until you've 
> waken up to find your hair cured in a block of cement.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry L. Munson
> Sent: Tuesday, March 11, 2008 3:24 PM
> To: [log in to unmask]
> Subject: Re: [TN] SV: [TN] disposal of alcohol/DI water solution
>
> We have a waste disposal company that uses the 5 gallons of collected IPA 
> water solution above 60 percent IPA to burn to make concrete.
>
> Terry Munson
> Foresite
> Sent from my Verizon Wireless BlackBerry
>
> -----Original Message-----
> From: Hfjord <[log in to unmask]>
>
> Date:         Tue, 11 Mar 2008 20:28:40
> To:[log in to unmask]
> Subject: [TN] SV: [TN] disposal of alcohol/DI water solution
>
>
> As far as I know, clean alcohol is not classified a poison. If you pour 
> some gallons a year in the wast water, the alcohol will be mixed in 
> proportions 1:trillions. Won't that be harmless? And DI is already water. 
> I'm not meaning to depreciate the laws, but sometimes I think we 
> exaggerate things.
> I had about half a litre of used acetone in a glass bottle in my lab. The 
> environmental inspection group made a raid one day and saw my bottle 
> without label. They ordered me to buy a special, explosion safe metal can, 
> pour the waste acetone in, and send the whole to an adress for 
> destruction. If not,they had the right to close my lab. I didn't argue 
> with them, took the bottle with the waste acetone to my home and found it 
> useful for this and that. Cheaper, faster, simpler. Am I a bad guy?
>
>
> Inge
>
> -----Ursprungligt meddelande-----
> Från: TechNet [mailto:[log in to unmask]] För Bev Christian
> Skickat: den 11 mars 2008 18:16
> Till: [log in to unmask]
> Ämne: Re: [TN] disposal of alcohol/DI water solution
>
> Phil,
> We bottle it in used IPA bottles (with new WHMIS labels - Canadian federal 
> protocol for chemicals) and then we have it removed by a bona fide waste 
> hauler.  Not sure what they do with this mixture, but for just spent 
> IPA/acetone/toluene (no water), it is burned for fuel.
> Bev
> RIM
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
> Sent: Tuesday, March 11, 2008 1:13 PM
> To: [log in to unmask]
> Subject: [TN] disposal of alcohol/DI water solution
>
> Hey Technetters,
>
> It just occurred to me that in using the alcohol/DI water mix for 
> determining the cleanliness of a circuit board, somewhere along the line 
> this becomes a waste fluid and needs to be disposed.  What are your 
> disposal methods?  I'm sure the local waste water folks would look poorly 
> on alcohol being added to the waste stream... unless it was Johnny Walker 
> Black or Stoli in their pockets.
>
> Phil Nutting
>
> Note: All the information contained in this e-mail and its attachments is 
> proprietary to Kaiser Systems, Inc. and it may not be reproduced without 
> the prior written permission of sender.  If you have received this email 
> in error, please immediately return it to sender and delete the copy you 
> received.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in the 
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per 
> day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential 
> information, privileged material (including material protected by the 
> solicitor-client or other applicable privileges), or constitute non-public 
> information. Any use of this information by anyone other than the intended 
> recipient is prohibited. If you have received this transmission in error, 
> please immediately reply to the sender and delete this information from 
> your system. Use, dissemination, distribution, or reproduction of this 
> transmission by unintended recipients is not authorized and may be 
> unlawful.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in the 
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per 
> day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives 
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in the 
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: 
> send e-mail to [log in to unmask]: SET Technet Digest Search the archives of 
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web 
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2