"Amol Kane (Asteelflash,US)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Amol Kane (Asteelflash,US)
Date:
Thu, 16 Aug 2012 06:33:38 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (28 lines)
Dear Technetters,

We are going to be assembling some lead-free  1.6x0.8 mm micro BGAs with
0.5mm pitch and 0.17mm dia board pads. Anybody else have experience with
this small a package?....I am concerned that there won't be sufficient
flux in the tiny solder deposit to clean the oxides during reflow,
leading to graping and/or head in pillow situation. Do I need a dip
fluxer for the part to do a flux only attachment, or to augment the
amount of flux in the solderpaste-solder bump system? I am told I have
no time to do DOEs to determine stencil and reflow parameters, so I am
turning to technet for help.....any thoughts?

 

 

Regards,

Amol

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2