TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 26 Mar 2001 12:11:03 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (55 lines)
Larry

Methylene chloride will not touch a well-cured epoxy resin, at least in
a reasonable time. If you remember, one of the standard cure tests for
solder resist is to rub it in one place with an MC-wetted white cloth
for a minute and see whether any colour has been transferred. If so, the
cure is not complete.

It is obtainable in most countries, though. In the USA, where the annual
consumption is about 400,000,000 lbs (180,000 tonnes), OSHA have
recently reduced its TWA PEL to 25 ppm and it does require reporting of
emissions under the TRI. It is certainly not the most benign solvent,
but it is probably not nearly as bad as it is painted. Some of its
substitutes, such as nPB (not suitable for paint stripping, BTW), are
probably far more dangerous, but are not regulated (yet!).

Brian

PS Please, Larry, do not use a bold font for your messages. The
easiest-to-read fonts are the plain text non-HTML types that your e-mail
client offers.

"Larry J. Fisher" wrote:
>
> The best stripping solvent I know of for cured epoxy materials is
> methlylne
> chloride. The best methlyene chloride "strippers" are the old paint
> strippers
> that contain methylene chloride and wax (when the methylene chloride
> starts
> to evaporate, the wax forms a barrier at the surface to prevent
> further
> evaporation - therefore the methylene chloride can strip further).
>
> Methlyene chloride is on the "bad news" list these days and is not
> easy to
> get. I'm not sure if you can even get the methylene chloride based
> paint
> strippers any more. Furthermore, the methylene chloride can also do a
> "number" on the butter coat of your laminate. Good Luck!
>
> Regards,
>
> Larry Fisher

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2