Larry Methylene chloride will not touch a well-cured epoxy resin, at least in a reasonable time. If you remember, one of the standard cure tests for solder resist is to rub it in one place with an MC-wetted white cloth for a minute and see whether any colour has been transferred. If so, the cure is not complete. It is obtainable in most countries, though. In the USA, where the annual consumption is about 400,000,000 lbs (180,000 tonnes), OSHA have recently reduced its TWA PEL to 25 ppm and it does require reporting of emissions under the TRI. It is certainly not the most benign solvent, but it is probably not nearly as bad as it is painted. Some of its substitutes, such as nPB (not suitable for paint stripping, BTW), are probably far more dangerous, but are not regulated (yet!). Brian PS Please, Larry, do not use a bold font for your messages. The easiest-to-read fonts are the plain text non-HTML types that your e-mail client offers. "Larry J. Fisher" wrote: > > The best stripping solvent I know of for cured epoxy materials is > methlylne > chloride. The best methlyene chloride "strippers" are the old paint > strippers > that contain methylene chloride and wax (when the methylene chloride > starts > to evaporate, the wax forms a barrier at the surface to prevent > further > evaporation - therefore the methylene chloride can strip further). > > Methlyene chloride is on the "bad news" list these days and is not > easy to > get. I'm not sure if you can even get the methylene chloride based > paint > strippers any more. Furthermore, the methylene chloride can also do a > "number" on the butter coat of your laminate. Good Luck! > > Regards, > > Larry Fisher --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------