Hi Technos,
I have a dynamite combination here. MEMS on PCBs that can be 0.093", 0.125" or even thicker. Currently the MEMS are in QFP package, but a castellated LCC is considered.
On top of it, the products are soon to be RoHS compliant.
It has been stated several times in this forum that leadless parts do not give reliable joints. But I have also seen castellated chips on aerospace boards. Are the castellated components more reliable than the plain leadless, where the joints are totally under the component?
Or otherwise stated, should I do my best to disqualify this package? Our application is maybe not high-rel, but just below, switching telecom devices.
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|