Subject: [TN] PWB measling and moisture
IPC 600 states that moisture content above 0.3% can lead to give rise to measling. I'm not so concerned about measling as I am deriving an acceptance limit for moisture in PWBs. My company is seeking a moisture acceptance level for PWBs. Can any of you explain the rationale for this 0.3% or is this arbitrary?
thank you, Mike Weekes
-----Original Message-----
From: George Milad [mailto:[log in to unmask]]
Sent: Monday, June 17, 2002 10:07 AM
To: [log in to unmask]
Subject: Re: [TN] ELni/au
Electroless Nickel /Immersion Gold (ENIG) has been tested extensively in a round robin study conducted by the IPC Plating Cimmittee 4-14.
The finish withstood more than 1.5 million actautions without any appreciable increase in resistance. This was published in a paper by G.Milad & G.OBrien in the proceedings fo the IPC fall meeting 2000 in Orlando FL and also in te IPC Review.
The committee recommends ENIG for this application.