TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Date:
Wed, 15 Nov 2006 15:48:08 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Hi Werner,



I don't know, to be honest. They do look deformed but I wouldn't to a significany extent. That is why I referred to their original size.



In addition, if the molten balls were in intimate contact with the paste I'd expect to see at least SOME coonection between the balls and the paste even if the paste never melt.



Regards,



Vladimir



-----Original Message-----

From: [log in to unmask]

To: Vladimir Igoshev; [log in to unmask]; [log in to unmask]

Sent: Wed Nov 15 15:37:15 2006

Subject: Re: [TN] More Separation in BGA joints



Hi Vladimir,

But how else would the balls deform?







Werner