TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 30 Jun 2006 09:28:39 +0800
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, don_well <[log in to unmask]>
Content-type:
text/plain; charset=gb2312
Subject:
From:
don_well <[log in to unmask]>
Content-transfer-encoding:
base64
Parts/Attachments:
text/plain (1 lines)
Hi All



  I recently faced a new issues with lead-free BGA.

  We use Qualcomm ICs in our productions. Recently Qualcomm's PCN shows the BGA balls material change from SAC305 to SAC105.The melting point update to 227 degree.

  Could you please tell me how to assembly the new BGAs, I mean which alloy paster should be used, SAC305 or other special? Any treatment should be made to the reflow profile?

  By the way what is the advancement of SAC105 alloy?