Hi Bill,
If the pads are laid out properly you can wave-solder SMD parts quite
successfully without chip wave. If you can't wave-solder the parts 'side-on'
to the wave due to design constraints, try wave-soldering the board at
different angles to the wave. A generous immersion depth helps too - easier
if you have a custom made board carrier. By the way, you might want to try
soldering at 465 degF instead of 500, you'll have less of a risk of
component damage and less dross too!!!
Regards,
Justin Braime
Process Engineer - Compuspec Industries
15a Vestey Drive, Mt Wellington
Auckland, New Zealand
[log in to unmask]
Ph: +64-9-574 1982
Fax: +64-9-574 1970
-----Original Message-----
From: Kasprzak, Bill (esd) US <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Sunday, April 18, 1999 12:29 AM
Subject: [TN] : Wave soldering CWR06 parts
>Tech-Netters:
>
>Anyone out there wave soldering CWR06 tantalum caps? Our design group has
>populated some of the larger case sizes on the back side of some boards. I
>didn't like this for a couple of reasons.
>
>#1 - The large case size will produce problems with "shadowing" since I do
>not have a chip wave.
>#2 - I didn't think that tantalum caps would survive the 500 degree F
plunge
>into the wave.
>
>Any comments on wavesoldering these parts?
>
>Any and all responses are welcome.
>
>Thanks,
>Bill Kasprzak
>Moog Inc.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|