Hi Earl,
Across an 18 x 24 panel, the minimum registration
tolerance of clearance to pad is +/- 0.002".
Isolated features can be
held to +/- 0.001" if essential.
We recommend a minimum solder mask web
width of 0.004". An absolute minimum of 0.0025"
can be maintained in isolated areas.
Hope this helps.
Best regards,
Keith Larson
Circuit Technology Inc.
[log in to unmask] wrote:
> I've been afronted with the latest BGA schemes dreamed up by someone not looking at, or willing to
> follow relatively simple design rules. That's my story.
>
> I remember LPI could hold fairly tight registration dimensions and tolerances across a panel. I just
> don't remember all I forgot concerning how tight these parameters might be.
>
> The best way to describe this dilemma is to say someone designed a 432 ball permiter BGA with some
> outer layer traces within 5 mils of the inside balls when 50 mils was available. With all things
> considered, without redesigning, there often are traces open to the aforementioned pads. Wonder why?
>
> The real question is what currently is reality without special "tweaking"? I mean, what are the
> practical process capability limitations concerning how tight will LPI S/M cover the distance
> without shorting - routinely - over say an 18 by 24 panel?
>
> Earl Moon
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
|
|
|