TECHNET Archives

May 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"McGlaughlin, Jeffrey A" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, McGlaughlin, Jeffrey A
Date:
Tue, 26 May 2015 10:29:06 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
http://quicksearch.dla.mil/

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Friday, May 22, 2015 12:15 PM
To: [log in to unmask]
Subject: Re: [TN] Solderability Dip Testing Device

So I got a recommendation to look at Mil-Std 202. Method 208.

Anyone have a link  to that free mil spec file site?

Rich  Kraszewski 
(920) 969-6075


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Thursday, May 21, 2015 8:37 PM
To: [log in to unmask]
Subject: [TN] Solderability Dip Testing Device

The link below describes an old school semi- automated dip device used for solderability testing :

https://www.ipc.org/TM/2.4.12a.pdf

The original citation  for this device came from a  now obsolete  Military soldering specification. 

Does anyone recall that mil spec document number?   I thought it might be in Mil Spec 28809 but I don't see it there. 

To cut to the chase,...  I seem to recall that military specification even mentioned a manufacturer. That is what I am ultimately looking for.

Any help would be appreciated. 

Thanks in advance

Rich  Kraszewski
Senior Process Engineer
Plexus Engineering Solutions 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2