Hans it's Ron from ITT:
Good point to bake if quantity/throughput allows. I had to do that a couple
times to get the preheat on machine with short preheat sections. Steve,
your flux will still be critical if you are using a low-residue VOC water
based stuff. RMA you will probably be ok. Baking works.
Ron
************************************
If this email is not intended for you, or you are not responsible for the
delivery of this message to the addressee, please note that this message may
contain ITT Privileged/Proprietary Information. In such a case, you may not
copy or deliver this message to anyone. You should destroy this message and
kindly notify the sender by reply email. Information contained in this
message that does not relate to the business of ITT is neither endorsed by
nor attributable to ITT.
************************************
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|