Lou:
I am not as versed as others on alloys, etc., however, like hand soldering
the tin can be burned up by heat. I would venture to say that heat may very
well be the answer. Werner, Dave Hillman, and you guys help me out here. I
would say that if you are taking solder samples and having them analyzed
that you can calculate your tin depletion rate. This depletion rate may be
affected by how much solder you need to add each day as to how much tin you
are actually depleting out of your pot. I think most of the solder
manufacturers have analysis labs that can analyze your samples. I believe
that there is also a table available in the IPC Standards, like MIL-Std 2000
document, that will inform you of acceptable tin depletion level.
Ron Hollandsworth
ITT
************************************
If this email is not intended for you, or you are not responsible for the
delivery of this message to the addressee, please note that this message may
contain ITT Privileged/Proprietary Information. In such a case, you may not
copy or deliver this message to anyone. You should destroy this message and
kindly notify the sender by reply email. Information contained in this
message that does not relate to the business of ITT is neither endorsed by
nor attributable to ITT.
************************************
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|