TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Date:
Fri, 13 Feb 2004 07:30:37 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bernard Kessler <[log in to unmask]>
Subject:
From:
Bernard Kessler <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"; format=flowed
Parts/Attachments:
text/plain (221 lines)
What happened to the old  .047" thickness??
Bernie Kessler





At 07:19 AM 02/13/2004 -0500, you wrote:
>Okay...  let me rephrase my question.  What would be the most common
>laminate thicknesses for double-sided FR-4 material, around the .045" range.
>I know that I can get .031 and .062 material, is there anything in between
>that would be considered "standard" (readily available without added cost)?
>
>Jim Marsico
>Senior Engineer
>Production Engineering
>EDO Electronics Systems Group
>[log in to unmask] <mailto:[log in to unmask]>
>631-595-5879
>
>
>         -----Original Message-----
>         From:   Scott B. Westheimer [SMTP:[log in to unmask]]
>         Sent:   Thursday, February 12, 2004 7:33 PM
>         To:     [log in to unmask]
>         Subject:        Re: [TN] FR-4 standard thickness
>
>         Roger,
>
>         "Standard" means different things to different people. IPC does not
>specify
>         standard thickness for double sided or multilayer PCB's, that is
>left up to
>         the product designer to meet their product  fit, form and functions
>needs.
>         What is normally considered is material availability as a industry
>standard.
>         Certainly 0.062" thickness, in a lot of cases is used for double
>sided and
>         boards are designed around that thickness. However some designs and
>products
>         can not be that thick and therefore other material needs to be used.
>
>         Scott Westheimer
>
>         Colonial Circuits
>         ----- Original Message -----
>         From: "Roger Stoops" <[log in to unmask]>
>         To: <[log in to unmask]>
>         Sent: Thursday, February 12, 2004 5:18 PM
>         Subject: Re: [TN] FR-4 standard thickness
>
>
>         Okay, I have a "newbie" type of question:
>
>         What are the "standard" thicknesses for double-sided boards?
>
>         And then the type of questions I ask when it's been a rough week:
>
>         Who determines the standard?  Has IPC determined a standard?
>
>         I would like to know so I can tuck it away in my quickly growing
>files of
>         pcb flotsam and jetsam...
>
>         Have a good one! (Time to call it a day)
>
>         Roger M. Stoops, CID+
>         Trimble Navigation Ltd., Dayton, OH, USA
>         Ph: +01 937.245.5288
>         Fax: +01 937.233.7511
>
>
>         -----Original Message-----
>         From: TechNet [mailto:[log in to unmask]]On Behalf Of Scott B.
>Westheimer
>         Sent: Thursday, February 12, 2004 3:48 PM
>         To: [log in to unmask]
>         Subject: Re: [TN] FR-4 standard thickness
>
>
>         James,
>
>         This is not a standard thickness if you are taking about a double
>sided PCB.
>         However if it is a multilayer and depending on how many layers it
>has it is
>         possible to get your required thickness. Most likely if you are
>talking
>         double sided than it will either be specially made by a laminate
>         manufacturer or the PCB fabricator. If the laminator makes it, it
>might be
>         expensive depending on the quantity needed.. It might be best to
>allow the
>         fabricator to make the material as it should cost less.
>
>         Scott Westheimer
>
>         Colonial Circuits
>         ----- Original Message -----
>         From: "Marsico, James" <[log in to unmask]>
>         To: <[log in to unmask]>
>         Sent: Thursday, February 12, 2004 3:04 PM
>         Subject: [TN] FR-4 standard thickness
>
>
>         > Good day Technet:
>         > Our designers are designing a PWB using IPC 4101/24 (FR406)
>material
>         that's
>         > .045" thick.  Is this a standard thickness that is readily
>available?
>         >
>         > Jim Marsico
>         > Senior Engineer
>         > Production Engineering
>         > EDO Electronics Systems Group
>         > [log in to unmask] <mailto:[log in to unmask]>
>         > 631-595-5879
>         >
>         > ---------------------------------------------------
>         > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>         > To unsubscribe, send a message to [log in to unmask] with following
>text in
>         > the BODY (NOT the subject field): SIGNOFF Technet
>         > To temporarily halt or (re-start) delivery of Technet send e-mail
>to
>         [log in to unmask]: SET Technet NOMAIL or (MAIL)
>         > To receive ONE mailing per day of all the posts: send e-mail to
>         [log in to unmask]: SET Technet Digest
>         > Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>         > Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>         for additional information, or contact Keach Sasamori at
>[log in to unmask] or
>         847-509-9700 ext.5315
>         > -----------------------------------------------------
>         >
>
>         ---------------------------------------------------
>         Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>         To unsubscribe, send a message to [log in to unmask] with following
>text in
>         the BODY (NOT the subject field): SIGNOFF Technet
>         To temporarily halt or (re-start) delivery of Technet send e-mail to
>         [log in to unmask]: SET Technet NOMAIL or (MAIL)
>         To receive ONE mailing per day of all the posts: send e-mail to
>         [log in to unmask]: SET Technet Digest
>         Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>         Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>         for additional information, or contact Keach Sasamori at
>[log in to unmask] or
>         847-509-9700 ext.5315
>         -----------------------------------------------------
>
>         ---------------------------------------------------
>         Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>         To unsubscribe, send a message to [log in to unmask] with following
>text in
>         the BODY (NOT the subject field): SIGNOFF Technet
>         To temporarily halt or (re-start) delivery of Technet send e-mail to
>         [log in to unmask]: SET Technet NOMAIL or (MAIL)
>         To receive ONE mailing per day of all the posts: send e-mail to
>         [log in to unmask]: SET Technet Digest
>         Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>         Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>         for additional information, or contact Keach Sasamori at
>[log in to unmask] or
>         847-509-9700 ext.5315
>         -----------------------------------------------------
>
>         ---------------------------------------------------
>         Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>         To unsubscribe, send a message to [log in to unmask] with following
>text in
>         the BODY (NOT the subject field): SIGNOFF Technet
>         To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>         To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>         Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>         Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
>or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>         -----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-----------------------------------------------------

Bernard Kessler & Associates, Ltd
714-898-8422  562-598-5563  Fx: 562-431-1741
www.home.earthlink.net/~bkesslerbka
       Service is our Profession

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2