TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kenneth Kirby <[log in to unmask]>
Date:
Sat, 29 Jan 2000 13:08:11 -0600
Content-type:
multipart/mixed; Boundary="0__=yrZHO5tDoKJu02wVNdChwx24MqIi4PwMI8ZgvO3v8uPCBzi6Mk9i0QVJ"
X-To:
Ivan Barrios <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kenneth Kirby <[log in to unmask]>
Parts/Attachments:
text/plain (1363 bytes) , pic30074.pcx (2490 bytes)



Unless you are concerned abour the Delta T of ceramic caps you should run
the solder temp at 280-500 degres F.  Yes, a low solder temperature will
result in skips and insufficient hole fill.

Ride The Wave,
Ken Kirby
Speedline Technologies



 (Embedded
 image moved   Ivan Barrios <[log in to unmask]>
 to file:      01/28/2000 02:21 PM
 pic30074.pcx)




To:   [log in to unmask]
cc:    (bcc: Kenneth Kirby/ElectrovertUS/Cookson)
Subject:  [TN] Wave solder pot twemperature




Is there a reccomendation on how hot the wave solder temperature should run
at
the pot/ We run at 450F and we are seeing some no solder on BSMT's is there
an
correlation in temperature vs no solders?
Thanks for any responses
Ivan Barrios

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################




ATOM RSS1 RSS2