We used a Proflow head for a couple of years back in 2000-2002 and
finally got rid of it. The head tended to plug up too often for our
liking. We made a custom aluminum spacer to put in the head to limit the
amount of solder in it so it would not dry out before we had to refill.
That improved the process but we ended up getting rid of the Proflow
head and went back to normal squeegees after a year of that. Hope this
helps.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Monday, May 01, 2006 2:02 PM
To: [log in to unmask]
Subject: [TN] Pump printing
Hi Technetters,
I wonder what your experiences are with this kind of technology, i.e.
Proflow head from DEK or Rheopump from MPM.
I have a high mix low volume application (250 different assemblies with
lot quantities between 5 and 20). The assemblies are ranging from low
complexity (a few SMT passives and an IC) up to fairly complex (10"x12",
high density, 0402, 10 mini BGAs).
Will a pump be good for me from the logistic/financial point of view?
What about the viability of these systems, are they OK, no tendency to
break whan you least need it?
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This e-mail has been scanned by MCI Managed Email Content Service.
______________________________________________________________________
This e-mail has been scanned by MCI Managed Email Content Service.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|