TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"PERALTA, Kevin (BREA)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 5 Jun 2001 09:40:30 -0400
Content-Type:
multipart/alternative
Parts/Attachments:
text/plain (3940 bytes) , text/html (8 kB)
Hey Joyce! Don't go to far out there. Remember "Inspect to Accept"! Since
there is only "Acceptable" criteria mentioned in the 610 document, I would
suggest to Steve to perform a dielectric resistance test to ease his mind.
Unless heat is going to be applied to the board again, the condition
probably won't progress.

Kevin L. Peralta
Senior Quality Systems Analyst
TRW Aeronautical / Lucas Aerospace


-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]]
Sent: Tuesday, June 05, 2001 5:35 AM
To: [log in to unmask]
Subject: Re: [TN] Measling...


I am no so sure...Steve is using polyimide board, which most likely is
for high reliability usage (not off the shelf items for commercial
usage)...I would not use it if it is for avionics (measling cross the
sky is scary...it may infect the stars...)..jk

-----Original Message-----
From: <Peter George Duncan> [mailto:[log in to unmask]]
Sent: June 4, 2001 10:23 PM
To: [log in to unmask]
Subject: Re: [TN] Measling...


No. The measling looks quite minor and doesn't come close to other
traces
or pads. Unless I'm mis-judging the scale of the picture, the affected
area
isn't carrying high power either, so I don't see that there's a problem.

Pete Duncan




                    "Stephen R.
                    Gregory"             To:     [log in to unmask]
                    <SteveZeva@AO        cc:     (bcc: DUNCAN Peter/Asst
Prin Engr/ST Aero/ST Group)
                    L.COM>               Subject:     [TN] Measling...
                    Sent by:
                    TechNet
                    <[log in to unmask]
                    ORG>


                    06/05/01
                    02:58 AM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    SteveZeva






Hi ya'll!

I took a few days off last week, and came back to be confronted with
some
boards that have been measled from rework...

Go to: http://stevezeva.homestead.com/index.html to take a peek.

The boards are polyimide, and it obviously appears that there was too
much
heat used when they were reworked...also they may have not been baked
prior

to the rework...I was told that they were, but you know how that goes.

I know what the -610 says about it, it says it's acceptable as long as
the
assembly performs as specified. There isn't any burns or anything around
any
of the barrels, just the measles...and it's only on one 14-pin DIP
location.
Would any of you have any REAL hesitation about accepting this assembly?

Thanks!

-Steve Gregory-

------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----


ATOM RSS1 RSS2