TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Tue, 6 Mar 2007 16:58:11 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
From:
Jeffrey Bush <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (133 lines)
Words of wisdom born from logic.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 37 
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/> 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Tuesday, March 06, 2007 3:52 PM
To: [log in to unmask]
Subject: Re: [TN] immersion silver and exposed copper in small vias

And what's wrong with exposed copper?  You certainly aren't going to try
and solder down there, are you?  Copper does not corrode quickly, and if
its going to be in a corrosive environment, you're going to have to
conformal coat anyway!

The silver is put on boards only to extend the solderability lifetime
of the bare copper, not as a protectant to prevent opens due to
corrosion.

This is not a reliability issue at all.

Wayne Thayer

>>> [log in to unmask] 3/6/2007 12:10:08 pm >>>
Hi Fran
The amount of mask intruding into the hole will depend on the
application method. Our curtain coat operation can cause the mask
(circa
1-2 microns) to penetrate about 1/3rd into the hole from both sides
but
it has not affected the silver taking on the remaining surface. Is the
mask too thick at the hole entrance to prevent the plating solution
getting good access?
You may also need to confirm by micro section what your customer
thinks
he is seeing. Is the mask covering all the hole surface? Hope this
helps.

Regards

Alistair

Alistair F Murray   MICT
Technical Manager
Artetch Circuits Limited
England UK
Direct Dial: 01903-712931

www.artetch.co.uk 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fran Juliot
Sent: 06 March 2007 15:58
To: [log in to unmask] 
Subject: [TN] immersion silver and exposed copper in small vias

Our customer is questioning what they feel is exposed copper in 8 mil
vias holes on silver boards.  We feel there is mask residue in the
holes
which does not allow silver to take.  These are holes that are allowed
to be plugged.  Has anyone else ran into this issue with thier
customers
and do you have the same look or are your small vias covered with
silver
all the way through the via?  

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2