TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Dan Skweres <[log in to unmask]>
Date:
Fri, 9 Mar 2007 12:18:27 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
From:
Jeffrey Bush <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (131 lines)
Not only when too small but also with excessive pressure - triangle
indents are witness marks from chisel probes at ET.

Jeffrey Bush

Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED 

           76 Technology Drive - POB 1890 

              Brattleboro, Vermont 05302

                Voice - 802.257.4571 ext 37 

                    Fax - 802.257.0011

                       <http://www.vtcircuits.com/> 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Skweres
Sent: Friday, March 09, 2007 11:16 AM
To: [log in to unmask]
Subject: Re: [TN] whodunit?

Sounds like you're on the right track. Chisel tip test probes whether
they were used at the bare board  test or at the assembly level more
than likely caused this. I've seen it happen at the bare board level
especially when the tip size is incorrect (too small) for the hole being
tested. It will push through the soft solder and into the hole exposing
the copper underneath.
Dan

>>> [log in to unmask] 03/09/07 09:39AM >>>
Hello Technet!
I've got a mystery today.  A colleague showed me a board, it's got some
unique damage on it.  It is the only one of maybe a thousand identical
assemblies, the rest do not have this damage.

Throughout the bottom side of the board there are damaged through-hole
pads.  The damage is an impact hole, where something triangular in shape
has in some cases literally punched through the pad.  In some cases
there is a lighter mark on the pad and/or on adjacent solder mask.  The
damaged pads are scattered throughout the board, they aren't restricted
to one area.  In some cases where there is damage there is visible
exposed copper.

Some facts
1) the board went through our assembly process without incident until
inspection
2) no unusual equipment malfunctions have been reported recently here -
so I don't think it is something we did.
3) The board is received with HASL finish on the pads, and is wave
soldered.
4) In all cases the damage is at a through-hole pad, some overlaps the
pad onto bare FR4/solder mask, but in all cases the damage at least
touches a pad.
5) the board also has SMT parts on the bottom side, we glue parts on
and wave solder attach them.  No damage has been identified on these
pads.

I'm concluding that:
- we don't have any equipment capable of doing this type of damage to
a PWB with such precision.
- because there is exposed copper, whatever happened likely took place
after HASL coating.

At this point my theory is that the electrical test at the PWB shop did
this, but it's a theory.  Can you PWB guys advise, is this possible? 
Where else would something triangular have the potential to whack the
pads?

As I said already, it's only one - but I hate an unsolved mystery! 
Please help.


regards,

Graham Collins
Process Engineer, 
L-3 Communications Electronic Systems Inc.
Halifax
(902) 873-2000 ext 6215

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2