TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Fri, 29 Aug 2003 08:55:23 -0400
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tom Gervascio <[log in to unmask]>
Subject:
From:
Tom Gervascio <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
Parts/Attachments:
text/plain (33 lines)
We started building product using these parts- QFN 32 (8 mm sq) and QFN


Motorola, National Semiconductor and Intersil all have useful
information on QFN. At a previous life, we found that extended the toe
to extend outside the periphery of the QFN package greatly assisted in
verifying solder deposition and reflow and also assisted in reworking
insufficient (we have vias in pad- another design flaw). We would run an
mini-wave tip around the periphery of the component.

The major problem we had was in printing thermal pads without
overprinting into thermal vias and getting insufficient solder.
According to National, you can have 80 % voiding in thermal pads without
sacrificing thermal dissipation.

would be interested in other's experiences

Tom Gervascio
Senior Process Engineer
Sparton Electronics
(352) 540-4040
[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2