TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Brian Ellis <[log in to unmask]>
Date:
Mon, 21 Feb 2000 11:56:12 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Kelly M. Schriver" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Kelly M. Schriver" <[log in to unmask]>
Parts/Attachments:
text/plain (144 lines)
Welcome back Charlie -

I agree 100% with Brian's words of caution, and would add a few of my own,
particularly if you have adhesives, sealants or conformal coatings to be
applied following assembly:

Verify the compatibility of each of these materials thru the entire
environmental range that your product must be subjected to.  I have
encountered some situations where the compatibility of the residues and the
coatings becomes a major problem, resulting in vessication and other messy
situations.

Regards - Kelly

-----Original Message-----
From: Brian Ellis <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Monday, February 21, 2000 9:19 AM
Subject: Re: [TN] THANKS and no clean info request


>Charlie
>
>Welcome back.
>
>I'm sure several responses may help you but, before you short-circuit
>all evaluation, please remember the two basic facts:
>
>1. Water-soluble chemistry gives you the widest operating window
>2. "No-clean" chemistry gives you a narrow operating window.
>
>This means that it is really impossible to just switch, as there are so
>many parameters to consider, e.g. solderability of boards and
>components, desired reliability of end product etc., etc., etc. Another
>point that it is important to realise: the term "no-clean" covers a
>multitude of sins and the easiest "no-clean" fluxes/pastes to use are
>those which are the most active and may leave the most active residues,
>causing future problems.
>
>I would therefore counsel caution in interpreting the responses to your
>enquiry. Caveat emptor.
>
>Brian
>
>Charles Barker wrote:
>>
>> Hello Technetters;
>>
>> As Steve Gregory let slip last week, I am back on the job. I'm somewhat
>> inundated with catching up, so I had not checked back in on TechNet right
away.
>>
>> MANY THANKS for all the prayers and good wishes. They were felt and very
much
>> appreciated by both my wife and me. I still have a good bit or soreness
from the
>> trauma of the surgery, but in general, I feel very good.
>>
>> Now back to the work/no clean thing:
>>
>> I am asking a BIGGG favor!
>>
>> I need to take a serious look at switching our process from a water
soluble flux
>> soldering operation to a no clean one. Normally, I would put several
cored wire
>> solders, liquid fluxes and solder pastes through a rigorous evaluation
process.
>> That could be considered re-inventing the wheel, since many of you have
probably
>> already done that.
>>
>> If any of you have done this and could share the results (OFF-LINE, of
course),
>> I would be greatly obliged.
>>
>> I would like to know which brands, which model numbers, which alloys and
under
>> what conditions they were tested, as well, of course, as the results.
>>
>> THANKS A BUNCH!!!
>>
>> Charlie B.
>> [log in to unmask]
>>
>> ##############################################################
>> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>> ##############################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
>> the body:
>> To subscribe:   SUBSCRIBE TECHNET <your full name>
>> To unsubscribe:   SIGNOFF TECHNET
>> ##############################################################
>> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>> information.
>> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
>> 847-509-9700 ext.5365
>> ##############################################################
>
>--
>Brian Ellis
>Protonique SA
>PO Box 78
>CH-1032 Romanel-sur-Lausanne, Switzerland
>Voice: +41 21-648 23 34 Fax: +41 21-648 24 11
>E-mail: [log in to unmask]
>URL: Technical and consultancy divisions:
>       http://www.protonique.com
>     Web services division:
>       http://www.protonique.com/webserv
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2