TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vg6sC-0000QUC; Fri, 3 Jan 97 04:29 CST
Old-Return-Path:
Date:
Fri, 3 Jan 1997 09:34:34 +0000
Precedence:
list
Resent-From:
From [log in to unmask] Fri Jan 3 08:
42:25 1997
Message-ID:
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/8931
TO:
Return-Path:
<TechNet-request>
X-Status:
Resent-Message-ID:
<"5cMs42.0.0DK.szDpo"@ipc>
Subject:
From:
Paul Gould <[log in to unmask]>
X-Loop:
In-Reply-To:
X-Mailer:
Turnpike Version 3.00 <o7n7tmQ9h8LB2OEq7S3FuLc$Ji>
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (42 lines)
In message <[log in to unmask]>, Todd Rogers
<[log in to unmask]> writes
>Technetters,
>We have been experiencing some sporadic problems with soldermask being
>burned off the edge of the circuits at the hot air level process.  The
>soldermask on the knee of the trace seems to burn off and allows the solder
>to stick to the trace edge.  We are using a chemical clean process prior to
>soldermask, and are spraying the soldermask on with a Teledyne spray
>coater.  Has anyone else experienced these problems and what did you do to
>fix it?
The soldermask must be too thin on the trace edges, (around 0.1 mil to casue
this problem). The amount of solder mask applied will depend on trace height and
distribution. Isolated traces are the most awkward as they tend to be overplated
realtive to the rest of the board and the ink has more room to flow off the
trace. You can only resolve this by increasing the amount of ink applied or
double coating.

I assume you are drying horizontally and that this problem is on both sides of
traces and not worse in X or Y directions. Bear in mind that as the ink is
heated in the intial drying phase, it will become less viscous and flow more if
held vertically.

We use curtain coating and the only answer for us to achieve 0.5 mil minimum
trace edge coverage on some boards is to double pass. One advantage of spray
coating is that a more thixotropic ink can be used to reduce flow. Curtain coat
ink by its nature has to be very runny. 
-- 
Paul Gould
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2