TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
R Sedlak <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Tue, 17 May 2005 06:14:42 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (190 lines)
Steve:   Do they spec out a Tin/Lead thickness, or whether the Tin/Lead should be reflowed?

Jeff Bush and I are really talking about two different kinds of finishes.   I have seen thin Tin/Lead, non-fused.  Could not fathom designing a board with this finish.   Jeff Bush is talking about Thick Tin/Lead, which is fused, not an easy board to build, but shelf life is not an issue.

Rudy Sedlak

Stephen Gregory <[log in to unmask]> wrote:
Hi Jeffery,

The board that I'm talking about doesn't seem to be that old
design-wise. So do you think that maybe the note is just something
kind of got "boiler-plated" from earlier designs?

A description of the board is that it is a VME styled board, and everything
on the board is SMT including headers, right angle push button switches,
etc., the only through-hole is two press-fit right angle connectors. So the
board is never going to see wave solder.

The board is 15-layers and only .065" thick. Do you think that maybe the
reason they have the note prohibiting HASL is because they don't want
to thermally shock the board which may cause other problems?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX


|---------+----------------------------->
| | Jeffrey Bush |
| | | | RCUITS.COM> |
| | Sent by: TechNet |
| | |
| | |
| | |
| | 05/17/2005 06:57 |
| | AM |
| | Please respond to |
| | TechNet E-Mail |
| | Forum; Please |
| | respond to Jeffrey|
| | Bush |
| | |
|---------+----------------------------->
>--------------------------------------------------------------------------------------------------------------|
| |
| To: [log in to unmask] |
| cc: |
| Subject: Re: [TN] SMOBC question... |
>--------------------------------------------------------------------------------------------------------------|




This process is called selective solderstrip and is incorporates
removing the tin/lead plating from masked areas, applying the mask then
reflowing the tin/lead plating to a solder finish. This is from a time
when HASL was new and not very robust - issues existed with the
thickness of the HASL deposit and problems were noted in assembly from
inadequate solder coating. The tin/lead reflow process offer a much
thicker solder alloy on the PCB and avoided the thickness issue. This
process worked best with hot-oil reflow as the tin/lead plating was
contaminated from photo resist development and when LPI was introduced,
mask developing.

I do not see this as an issue today with a well controlled HASL process.

Jeffrey Bush
Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com


-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: Monday, May 16, 2005 7:50 PM
To: [log in to unmask]
Subject: [TN] SMOBC question...

This may seem like a strange question, but here it is:

Can a board have a tin/lead finish on the solderable surfaces when
SMOBC is called out, and comply with a note on the drawing that
SPECIFICALLY states that HASL is not allowed?

I have a fab vendor that's telling me that it's not possible. SMOBC
without
HASL can't happen, if you want a tin/lead finish on the pads...is that
true?

I've been told that there will be some areas that will wind-up having a
tin/lead
finish beneath the soldermask, which we all know isn't a good thing
because
of the loss of adhesion of the mask when the assembly goes thru reflow
or
wave solder.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc. It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message
and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------
Yahoo! Mail

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
 Stay connected, organized, and protected. Take the tour

ATOM RSS1 RSS2