TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Geoff Layhe of Lamar Group <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Geoff Layhe of Lamar Group <[log in to unmask]>
Date:
Fri, 16 Sep 2005 12:40:05 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (147 lines)
Looks like there's still delamination, specially noticeable on "bake 2". I'd guess that the problem is one of adhesion rather than cure. 

Geoff Layhe

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Gregory
Sent: Friday, September 16, 2005 12:17 PM
To: [log in to unmask]
Subject: Re: [TN] Rework for Delaminated PWBs


Mornin' Everybody!

I have the pictures that Mumtaz sent me posted now. Go to:

http://www.stevezeva.homestead.com  and click on "Picture Page 2"
and look at; "Blister 1, Blister 2, After Bake 1, and After Bake 2".

Boy, that's some SERIOUS delamination! I don't know enough to say
if the rework that your supplier is proposing is acceptable, but my first
question would be is why would they send you boards that are not cured?

If they sent you boards that are that undercured, what else is wrong with
these boards?

I would have a very hard time accepting these boards. Which brings up
another question, if you say you won't accept them and that you want new
boards, how will you know that you won't get the same boards that your
supplier has "reworked"?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX




                      Mumtaz Bora
                      <mbora@KYOCERA-WI        To:       [log in to unmask]@SMTP@Exchange
                      RELESS.COM>              cc:       (bcc: Stephen R Gregory/LABARGE)
                      Sent by: TechNet         Subject:  [TN] Rework for Delaminated PWBs
                      <[log in to unmask]>


                      09/15/2005 08:20
                      PM
                      Please respond to
                      TechNet E-Mail
                      Forum
                      <[log in to unmask]>
                      ; Please respond
                      to Mumtaz Bora
                      <mbora@KYOCERA-WI
                      RELESS.COM>





Dear Technetters,


We have received a large batch of PWBs that is showing delamination after
reflow at peak temp. 230C. Laminate is high Tg - 170C.

Supplier is proposing to perform the following rework -- on these boards
instead of providing replacement parts.

  Oven bake at 190C for 2.5 hours followed by second bake at 150C for 2
hours at 6kg/cm2 pressure. Will this guarantee a full cure?

I am concerned about latent failures and layers opening up as full cure was
not achieved the first time.

Any inputs from the forum will be appreciated.

I will request Steven Gregory to place the image of delamination on his
website.  Have a great weekend.
Thank-you

Mumtaz

  D/ 252 - SMT Process and Component Quality
  Bldg. V238E
Voice  (858)-882-1967
Fax    (858)-882-3126
Page  (858)-635-1180
Cell:   (858) -449-7054
email: [log in to unmask]
Kyocera-Wireless Corp.
10300, Campus Point Drive

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
San Diego, Ca  92121,USA



__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

Private & Confidential:

This e-mail message is confidential and is intended solely for the person or organisation to whom it is addressed.  If the message is received by anyone other than the addressee please return the message to the sender by replying to it and then delete the message from your computer.

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2