It makes a difference what kind of solder you use. If you use special low
drossing solder, you won't benefit, because the Kleenox will pull out the
organics, mainly the Phosphorous in your low drossing solder, then you'll
be back where you come from. Kleenox will benefit you if you have
intentions of using less fresh solder to replenish your pot; However,
downtime may or may not be reduced.
"Moss, Thomas" <[log in to unmask]> on 08/03/98
04:28:00 PM
Please respond to "TechNet E-Mail Forum."
<[log in to unmask]>; Please respond to "Moss,
Thomas" <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Jason Smith/Lex/Lexmark)
bcc: Jason Smith/Lex/Lexmark
Subject: [TN] Questions about KLEENOX "P"
Hello all,
I've been lurking on the list for awhile, but I thought I'd come
out of hiding to ask some questions.
I want to try some Kleenox "P" to reduce the amount of dross
from our Wave Solder pot. Does anyone out there have any good or bad
experiences with its use? Will its repeated use leave a residue or
contamination in the solder? Are there any downsides that I'm not
thinking of? Lastly, was it cost-effective for you to use?
Thanks in Advance,
Tom Moss
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|