TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Thu, 20 Dec 2001 17:30:40 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
From:
Mel Parrish <[log in to unmask]>
Parts/Attachments:
text/plain (265 lines)
Hi Jim!
Didn't find it on the site, but IPC is fixin (Alabamese) to put it on. In
fact it may be there by time this is posted.  It is also attached.

Mel Parrish
Soldering Technology International
Madison, AL
256 705 5530
256 705 5538 Fax
[log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Marsico, James
Sent: Thursday, December 20, 2001 3:51 AM
To: [log in to unmask]
Subject: Re: [TN] Mil Spec Equivalent for IPC-A-610


Is the adoption notice available on the IPC web site?

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879



        -----Original Message-----
        From:   Mel Parrish [SMTP:[log in to unmask]]
        Sent:   Wednesday, December 19, 2001 6:31 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] Mil Spec Equivalent for IPC-A-610

        Hans
        Depending on the exact year, the 454 (Requirement 5?) reference
could be to
        any number of standards including WS-6536 or 45743, but you are very
correct
        they were eliminated without any identified replacement.  J-STD-001
has a
        recent DoD adoption notice that I can send if you like, or you can
get it
        from IPC directly.

        Mel

        -----Original Message-----
        From: TechNet [mailto:[log in to unmask]]On Behalf Of Hinners Hans M
Civ
        WRALC/LUGE
        Sent: Wednesday, December 19, 2001 1:08 PM
        To: [log in to unmask]
        Subject: Re: [TN] Mil Spec Equivalent for IPC-A-610


        Hello Fellow Techies,

        Thanks for the comments!

        The original drawings are from the late 80's and we're conformally
coating
        the assembly instead of using an insulating foam so I get to
change/improve
        things.
        MIL-STD-2000 came out after the drawings (which reference
MIL-STD-454).  And
        then there's the disconnect when both specs got canceled without an
        identified replacement.  I'd rather identify a non-government
specification
        supporting DOD's decision to get out of the spec. business.  (They
had
        better solder the thing to J-STD-001 or I've got bigger problems
than
        getting a good coating.)

        Happy Holidays.

        Hans

        Integrity First  -  Service Before Self  -  Excellence in All We Do
        ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
        Hans M. Hinners
        Electronics Engineer
        Warner Robins - Air Logistics Center (WR-ALC/LUGE)
        226 Cochran Street
        Robins AFB GA 31098-1622

        mailto:[log in to unmask]

        Com: (478) 926 - 5224
        Fax:   (478) 926 - 4911
        DSN Prefix: 468



        -----Original Message-----
        From: Mel Parrish [mailto:[log in to unmask]]
        Sent: Wednesday, December 19, 2001 5:10 PM
        To: [log in to unmask]
        Subject: Re: [TN] Mil Spec Equivalent for IPC-A-610


        Hans
        The only standard from the Mil specs that expressly addressed
acceptability
        like 610 was the DOD-STD-2000, Volume 3.  The other standards like
        MIL-STD-2000 and 2000, Rev A included acceptability as would be
equivalent
        to J-STD-001.

        Mel Parrish
        Soldering Technology International
        Madison, AL
        256 705 5530
        256 705 5538 Fax
        [log in to unmask]


        -----Original Message-----
        From: TechNet [mailto:[log in to unmask]]On Behalf Of Hinners Hans M
Civ
        WRALC/LUGE
        Sent: Wednesday, December 19, 2001 11:42 AM
        To: [log in to unmask]
        Subject: [TN] Mil Spec Equivalent for IPC-A-610


        Hi All,

        Can anyone remember the equivalent Mil spec for IPC-A-610?
        Is it MIL-STD-454?

        Hans

        Integrity First  -  Service Before Self  -  Excellence in All We Do
        ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
        Hans M. Hinners
        Electronics Engineer
        Warner Robins - Air Logistics Center (WR-ALC/LUGE)
        226 Cochran Street
        Robins AFB GA 31098-1622

        mailto:[log in to unmask]

        Com: (478) 926 - 5224
        Fax:   (478) 926 - 4911
        DSN Prefix: 468


----------------------------------------------------------------------------
        -----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET
        Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
        E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
        ext.5315

----------------------------------------------------------------------------
        -----


----------------------------------------------------------------------------
        -----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET
        Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
        E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
        ext.5315

----------------------------------------------------------------------------
        -----


----------------------------------------------------------------------------
        -----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET
        Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases >
        E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
        ext.5315

----------------------------------------------------------------------------
        -----


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2