TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w1xfb-0007zXC; Tue, 4 Mar 97 11:06 CST
Encoding:
14 TEXT
Old-Return-Path:
Date:
Tue, 4 Mar 1997 09:20:55 -0800
Precedence:
list
Resent-From:
Cc:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10831
From [log in to unmask] Wed Mar 5 14:
39:22 1997
TO:
"'Ed Cosper'" <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"YyxfG1.0.8lH.EQ57p"@ipc>
Subject:
From:
"Davis, Mary" <[log in to unmask]>
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Mailer:
Microsoft Exchange Server Internet Mail Connector Version 4.0.994.63
Message-ID:
Parts/Attachments:
text/plain (27 lines)
Concerning the 2.0 microgram/sq. in. limit:
Mark Shireman of Alliant Techsystems just presented a paper at China
Lake about a military low residue soldering production process.  Based
on their experience, he recommends a bare board limit of < 2.0
micrograms/sq.in. for most designs.  The data was generated using an
Omegameter 600SMD, 10 minute cycle, unheated. I think the limit
originated from a study conducted for the Army by Contamination Studies
Laboratory. 

Mary Davis
Hughes Aircraft
Naval & Maritime Systems
206-356-3311
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2