Hello Iain,
Story sounds familiar here, although not so catastrophic...
BGA material change might be the explanation: lead-free BGAs are
designed to withstand hotter reflow profiles and use more thermally
resistant materials like molding compounds and die attach glue. This has
a direct impact on the warpage orientation and value.
Note also that your specific daisy-chained component has a small die
size compared to the BGA dimensions, which is un favourable in terms of
warpage (check with X-Ray).
Question: Was your refow profile a SnPb, SAC or an hybrid one?
Hope this helps.
A. Grivon
Braddock, Iain a écrit :
> Techies, need a little help here!
>
> In preparation for assembling some development boards with an 1152 PBGA, I purchased some Practical Components dummy boards & devices double sided ENIG and 1156 PBGA'. I took the opportunity to get 63/37SnPb and leadfree (SAC 305) BGA's which are identical in sized. Alloy comfirmed by XRF.
>
> The evaluation boards (PCB012) amongst others had footprints for 2 off 1156 devices, so populated 1 off each component per board.
>
> I asked TSL (UK) to provide a stencil with their recommendations and ended up with a 0.005" S/S laser cut with 0.0005" aperture reduction.
>
> The paste used was our standard multicore 62/36/2 SnPbAg
>
> The reflow profile peaked @ 232C with time above liquidus for, 1) SAC - 29 secs 2) SnPb - 74 secs.
>
> Now comes the fun bit:
>
> Post reflow the SAC BGA had a stand off of 0.4mm in the centre (sides) but less in the corners ie. curled down, and all 4 corners with solder bridges.
> The 63/37 BGA had a stand off of ~ 0.5mm but this time at the 4 corners with slightly less in the middle (I crudely used feeler gauges!)
>
> So it would appear that one BGA curled up and the other curled down....with different amounts of collapse.........hmm?
>
> Anyone provide an explanation of this phenomenon?
>
> CIA,
> Iain.
>
>
>
> ********************************************************************
> This email and any attachments are confidential to the intended
> recipient and may also be privileged. If you are not the intended
> recipient please delete it from your system and notify the sender.
> You should not copy it or use it for any purpose nor disclose or
> distribute its contents to any other person.
> ********************************************************************
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|