Hello Corey,
It is recommended that you not solder over a gold thickness of 30 uins, you
will have gold embrittlement caused by the AuSn, intermetallic. If however,
you reduced the gold thickness to < 10 uins, the solder joints will be
stronger, with soldering to the nickel, beneath, occuring.
Regards,
Lenny Kurup
EMX Enterprises Ltd.
On Mon, 27 Apr 1998, Cory and Lise Steeby wrote:
> We are evaluating a fully gold plated (30uin) connector for a new product.
> I have heard that soldering a gold plated connector to a PCB can cause a
> brittle solder joint because of the intermetallic bonds made between the
> gold and solder. The assembly is through-hole and wave soldered. Gold
> plating is required of the contact portion of the connector because of
> environment and signal levels. I am trying to weigh the gold contact pro
> against the gold solder joint con.
>
> Can anyone verify this or point me to evidence that this is not a problem?
>
> Thank You
>
> Cory Steeby
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|