TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
SteveZeva <[log in to unmask]>
Date:
Tue, 26 May 1998 14:55:34 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Lenny Kurup <[log in to unmask]>
Subject:
From:
Lenny Kurup <[log in to unmask]>
In-Reply-To:
Content-Type:
TEXT/PLAIN; charset=US-ASCII
MIME-Version:
1.0
Parts/Attachments:
TEXT/PLAIN (60 lines)
Hi All,

The issue of exposed copper, and subsequent oxidation, for an electronic
application, is very important, not only from a joint defect point of view
but, also from a trace conductor viewpoint. A typical trace and/or pad is
built with a design for a minimum conduction amount, both heat and
electrical characteristics are calculated based on a thickness of
copper. Alter the copper thickness and/or purity, by oxidation for
instance, and you alter the characteristics of the circuit, which may lead
to subsequent field failures.

LK

On Tue, 26 May 1998, SteveZeva wrote:

> Hi Nicolas!
>
>      As far as the exposed copper that results from an OSP process, there
> isn't an issue as far as I know. Yes the copper will oxidize, but from the
> little bit I know about metallurgy, it's my understanding is that the copper
> will be coated with a layer of oxidation, and then it slows down dramatically.
> For a illustration of that just think about some of the copper water lines in
> old houses, the copper telephone lines exposed to the elements for years and
> years...that shows that it takes quite a while for copper to deteriorate.
>
>      Somebody correct me if I'm wrong about this, but the exposed copper
> problems that are defects usually have something to do with the exposed copper
> being an indicator of some other problem, not the fact that the copper itself
> is exposed. Oxidation of the copper is normally only a problem when trying to
> solder to it...
>
> C-ya,
>
> -Steve Gregory-
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2