TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wHajb-000BjFC; Wed, 16 Apr 97 14:51 CDT
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Wed, 16 Apr 1997 13:00:40 -0700 (PDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12041
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"ND8h61.0.ZMM.jsILp"@ipc>
Subject:
From:
Bill Marsh <[log in to unmask]>
Mime-Version:
1.0
From [log in to unmask] Wed Apr 16 15:
44:42 1997
X-Loop:
Message-Id:
<v03007802af7a7dfeb415@[128.102.146.157]>
Parts/Attachments:
text/plain (51 lines)
>
>To: VAN HOREN EDUARD VM81 014 57 20 08 <[log in to unmask]>
>From: Bill Marsh <[log in to unmask]>
>Subject: Re: VIAS IN 0805 PADS WAVESOLDERING
>Cc:
>Bcc:
>X-Attachments:
>
>Check  IPC-SM-782, which has guidelines about via and pad design.
>
>>Hi,
>>Like everybody (?) we are using 0805 components in wavesoldering.
>>When there is a viahole in the pad, we see a number of very thin
>>solderjoints (almost undetectable visually) and even non-soldered
>>components.
>>Is there an experience in the field about allowing or not allowing this
>>configuration, and about via-hole size and via-position in the pad to
>>reduce or prevent defects ?
>>Eddie Van Horen  [log in to unmask]
>>
>>
>>***************************************************************************
>>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>>***************************************************************************
>>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
>>* with <subject: subscribe/unsubscribe> and no text in the body.          *
>>***************************************************************************
>>* If you are having a problem with the IPC TechNet forum please contact   *
>>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>>***************************************************************************
>
>
>

Bill Marsh
Phone: 415-604-6979
e-mail: [log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2