TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 9 Nov 2006 20:17:47 -0600
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
From:
Jack Olson <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
I would have guessed Latin.

but on a whim, I googled
"curiosum aurorum"
and got exactly one hit.

ONE HIT ???

usually my searches return closer to a bazillion!

(and it was some kind of crypto crackin' dictionary)

curiosumer and curiosomer,

jbro



----- Original Message -----
*Date:*         Thu, 9 Nov 2006 12:23:10 -0800
*Reply-To:*     TechNet E-Mail Forum <[log in to unmask]>,
              JaMi Smith <[log in to unmask]>
*Sender:*       TechNet <[log in to unmask]>
*From:*         JaMi Smith
<[log in to unmask]><http://listserv.ipc.org/scripts/wa.exe?A2=ind0611&L=technet&D=0&T=0&P=24705>
*Subject:*      Re: Gold Embrittlement
*X-To:*         TechNet E-Mail Forum <[log in to unmask]>
*Content-Type:* text/plain; charset="iso-8859-1"


Richard,


Guessing at the definition of "curiosom aurorum", or even the language, is
very likely to get me into even deeper trouble with the forum than I am now,
but I would assume that it is a "curiosity" of some sort, and if that is the
case, then I certainly would be willing.


As I see it, participating in a forum like this (and by participating I mean
participating in the dialogue, and not just reading the posts) is somewhat
like sticking your neck out, and you can't do that without someone
occasionally cutting it off.


JaMi

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2