TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
James Mahoney <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, James Mahoney <[log in to unmask]>
Date:
Fri, 3 Apr 2009 12:43:58 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (84 lines)
What's the surface finish you are dealing with? Some hard gold plating lines
could handle assembled boards depends on the board configuration. I would
think removing the current surface finish will be the biggest challenge.


Please update your contact for Jim Mahoney
[log in to unmask]
Thank you, 
Jim Mahoney 
Quick Turn Flex Circuits, LLC 
Applications Project Manager 
P# 603-821-6571 
F# 603-821-5723 
M# 603-305-6250 

** This email and all attachments have been scanned prior to being sent** 
Confidentiality Notice: This page and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure and
is intended for the exclusive use of the addressee. If you are not the
intended recipient, you are hereby notified that any disclosure, copying,
distribution or use of the contents of this information in any manner is
strictly prohibited.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gary Camac
Sent: Friday, April 03, 2009 12:39 PM
To: [log in to unmask]
Subject: [TN] Edge connector repair

Good morning all,

 

Here's the scenario - I have assemblies that should have Ni/Au plating
on edge connector but don't; the assemblies are built; can repairs be
made?

 

Thanks in advance, 

 

Gary Camac

Senior Manufacturing Engineer

DICKEY-john Corp.

5200 Dickey John Road

Auburn, IL 62616-0010

Telephone 217-438-2288

[log in to unmask]

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2