TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dwight Mattix <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dwight Mattix <[log in to unmask]>
Date:
Thu, 20 Jan 2005 14:32:58 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (97 lines)
Scott,
The approach you describe is lower risk application for Silver
contact.  The contact only has electrical bias applied at the moment of
switch contact.

dw

At 11:56 AM 1/20/2005, Roger Stoops wrote:
>Scott,
>
>On some of our products we built some years ago we used carbon as an
>alternate for Au for LCD and switch contacts.  We had no reported
>problems, either from assembly or the end-user.
>
>Dwight made a good point in his email.  Interesting side point to his
>comments: when we needed to build our own keypad, the contact layer was
>silver on mylar sealed to a pcb with PSA adhesive (pcb contacts were
>ENIG).  Even though there were no apparent openings and no vents, to our
>dismay the contacts oxidized rather quickly (found sulfur and moisture in
>enclosed areas).  The vendor suggested a thin layer of carbon ink over the
>silver.  Worked like a charm.  You may find it helpful to find out what
>ink your vendor is using and specify it on your print.
>
>Question for anyone: Has anyone used IAg as a board finish with carbon ink
>over any desired areas?  Seems like it might work for a keypad with parts
>on one side and contacts on the other...
>
>Rgds,
>
>Roger
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Scott Lefebvre
>Sent: Thursday, January 20, 2005 2:37 PM
>To: [log in to unmask]
>Subject: [TN] Carbon Keypad
>
>
>Currently we use gold for all of our keypads.  I want to reduce the cost
>of a product and thought about switching to a carbon keypad.  I am not
>familiar with the process and wanted to know a few things.  We mostly use
>a water-soluble process and our entire product is washed.  Some boards are
>a mixed technology using SnPb currently.
>
>?  Are there any Reflow solder concerns I should be aware of?
>?  Are there any Wave solder concerns I should be aware of, like masking
>pads during wave solder?
>?  Are there any other concerns period that I should be addressing.
>
>Thank you,
>
>Scott
>
>
>
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2